Feadánra Cruach Dhosmálta ASTM A269 TP304

Feadánra Cruach Dhosmálta ASTM A269 TP304



1. Caighdeán: ASTM A269, ASME SA269
2. OD: 6.0mm -500.0mm
3. Tiús Balla: 0.6mm -12.7mm
4. Fad: Fad Randamach Aonair, Fad Randamach Dúbailte agus Saincheaptha
Glaoigh Linn
Réamhrá Táirgí

Feadánra Cruach Dhosmálta ASTM A269 TP304tá friotaíocht creimeadh an-ard, inphróiseasacht maith agus infheictheacht. An raon teochta is infheidhme deFeadán gan uaim ASTM A269 GR TP304idir -325 céim F agus 1500 céim F (-198 céim go 816 céim), agus is féidir leis teocht ard agus coinníollacha foircneacha a sheasamh. Dá bhrí sin,cóimhiotal 304is féidir é a úsáid i dtimpeallachtaí creimneach teocht ard ar nós uisce, oxidants, aigéid agus alcailí. Is soláthraí píopa cruach dhosmálta í ár gcuideachta a bhfuil 15+ taithí easpórtála aige. Déan teagmháil linn le haghaidh tuilleadh eolais agus luachan saor in aisce!

 

Caighdeán Feadáin Cruach Dhosmálta ASTM A269 TP304:

  • ASTM A269: Sonraíocht Chaighdeánach le haghaidh Feadáin Cruach Dhosmálta Austenític Gan uaim agus Táthaithe le haghaidh Seirbhíse Ginearálta

 

  • ASTM A249: Sonraíocht Chaighdeánach le haghaidh Coirí Cruach Austéiníteacha Táthaithe, Sárthéitheoir, Malartóir Teasa, agus Feadáin Comhdhlúthadáin

 

  • Gráid: 316, 316L, 316Ti, 316L Mod, 17-4ph, 310, 310S, 317, 317L, 321, 321H, 347, 347H, 904L, 254SMO, 235MA05, S S31803, 2507, S31050, S30815, Etc.
ASTM A269 TP304 stainless steel tubing suppliers

Sonraíocht Tube ASTM A269 TP304

Sonraíocht ASTM A269, ASME SA269
Cruthanna Hiodrálacha, Babhta, Cruth U, Coiled
Cineál Déantúsaíochta Déanta / Gan uaim / ERW / EFW / Táite
Críochnaigh Dromchla BA, 2B, Uimh.8, Uimh.1, Uimh.4, Uimh.3, 8K, 2D, 1D, HL, 400G
Raon Tiús SCH XXS, SCH 10, SCH XXH, SCH 5, SCH 40, SCH XS, SCH 80S, SCH 160, SCH 80
Teicníc Fuar tharraingt, Fuar-rollta, Easbhrúite, Hot rollta Tube
Caighdeán ASTM, GB, DIN, JIS, AISI, GA, SUS
CRÍOCH Deireadh Beveled, Treaded, Deireadh Gnáth
Seirbhís Próiseála Gearradh, Decoiling, Lúbthachta, Táthú, Punching, Mhúnlú
Coinníoll Seachadta Snasta, Fuar Tarraingthe, Annealed agus Piocáilte (AP), MF, Geal Annealed (BA)
Pacáil Muinchille, Boscaí Adhmaid, Críochnaíonn Teorainneacha

Déan teagmháil anois

Feidhmchlár Feadánra Cruach Dhosmálta ASTM A269 304

  • Peitriceimiceach
  • Bia
  • Cógaisíochta
  • Aeraspáis
  • Réimse cosanta comhshaoil
  • leathsheoltóir
  • Innealra beachtais

 

Feidhmíocht Próiseála Feadáin SS 304

Is féidir 1.4301 304 píopa cruach dhosmálta a phróiseáil trí easbhrúite, líníocht fuar, rollta fuar agus lúbadh fuar chun freastal ar riachtanais cruthanna casta éagsúla.

 

AISI 304 Soláthraí Feadáin Dhosmálta

Is soláthraí agus monaróir gairmiúil cruach dhosmálta ASTM A269 UNS S30400 é HT PIPE. Soláthraímid freisin 304 feistis cruach dhosmálta, flanges, dúntóirí, píopaí, feadáin, plátaí, leatháin, stiallacha, slata, etc.

 

Rátáil Brú Feadán ASME SA269 TP304

Balla Tiús in orlach Trastomhas Amuigh san Inse Íos-neart teanntachta (PSI) Neart Íostairbhe (PSI) Brú Oibre Brú Pléasctha Teoiriciúil Pointe Torthúil Teoiriciúil Laghdaigh Brú
0.020 0.250 75,000 30,000 3,571 14,286 5,714 4,416
0.028 0.250 75,000 30,000 5,412 21,649 8,660 5,967
0.035 0.250 75,000 30,000 7,292 29,167 11,667 7,224
0.049 0.250 75,000 30,000 12,089 48,355 19,342 9,455
0.065 0.250 75,000 30,000 20,313 81,250 32,500 11,544
0.020 0.375 75,000 30,000 2,239 8,955 3,582 3,029
0.028 0.375 75,000 30,000 3,292 13,166 5,266 4,145
0.035 0.375 75,000 30,000 4,303 17,213 6,885 5,077
0.049 0.375 75,000 30,000 6,634 26,534 10,614 6,816
0.065 0.375 75,000 30,000 9,949 39,796 15,918 8,597
0.020 0.500 75,000 30,000 1,630 6,522 2,609 2,304
0.028 0.500 75,000 30,000 2,365 9,459 3,784 3,172
0.035 0.500 75,000 30,000 3,052 12,209 4,884 3,906
0.049 0.500 75,000 30,000 4,571 18,284 7,313 5,304
0.065 0.500 75,000 30,000 6,588 26,351 10,541 6,786
0.083 0.500 75,000 30,000 9,319 37,275 14,910 8,307
0.020 0.625 75,000 30,000 1,282 5,128 2,051 1,859
0.028 0.625 75,000 30,000 1,845 7,381 2,953 2,568
0.035 0.625 75,000 30,000 2,365 9,459 3,784 3,172
0.049 0.625 75,000 30,000 3,487 13,947 5,579 4,335
0.065 0.625 75,000 30,000 4,924 19,697 7,879 5,591
0.083 0.625 75,000 30,000 6,781 27,124 10,850 6,910
0.095 0.625 75,000 30,000 8,190 32,759 13,103 7,734
0.109 0.625 75,000 30,000 10,043 40,172 16,069 8,639
0.028 0.750 75,000 30,000 1,513 6,052 2,421 2,156
0.035 0.750 75,000 30,000 1,930 7,721 3,088 2,669
0.049 0.750 75,000 30,000 2,818 11,273 4,509 3,664
0.065 0.750 75,000 30,000 3,931 15,726 6,290 4,749
0.083 0.750 75,000 30,000 5,330 21,318 8,527 5,905
0.095 0.750 75,000 30,000 6,362 25,446 10,179 6,637
0.109 0.750 75,000 30,000 7,683 30,733 12,293 7,453
0.120 0.750 75,000 30,000 8,824 35,294 14,118 8,064
0.020 0.875 75,000 30,000 898 3,593 1,437 1,340
0.028 0.875 75,000 30,000 1,282 5,128 2,051 1,859
0.035 0.875 75,000 30,000 1,630 6,522 2,609 2,304
0.049 0.875 75,000 30,000 2,365 9,459 3,784 3,172
0.065 0.875 75,000 30,000 3,272 13,087 5,235 4,126
0.083 0.875 75,000 30,000 4,390 17,560 7,024 5,152
0.095 0.875 75,000 30,000 5,201 20,803 8,321 5,807
0.109 0.875 75,000 30,000 6,221 24,886 9,954 6,543
0.120 0.875 75,000 30,000 7,087 28,346 11,339 7,100
0.028 1.000 75,000 30,000 1,112 4,449 1,780 1,633
0.035 1.000 75,000 30,000 1,411 5,645 2,258 2,027
0.049 1.000 75,000 30,000 2,037 8,149 3,259 2,796
0.065 1.000 75,000 30,000 2,802 11,207 4,483 3,647
0.083 1.000 75,000 30,000 3,732 14,928 5,971 4,567
0.095 1.000 75,000 30,000 4,398 17,593 7,037 5,159
0.109 1.000 75,000 30,000 5,227 20,908 8,363 5,827
0.120 1.000 75,000 30,000 5,921 23,684 9,474 6,336
0.134 1.000 75,000 30,000 6,865 27,459 10,984 6,963
0.035 1.250 75,000 30,000 1,112 4,449 1,780 1,633
0.049 1.250 75,000 30,000 1,595 6,380 2,552 2,260
0.065 1.250 75,000 30,000 2,176 8,705 3,482 2,958
0.083 1.250 75,000 30,000 2,871 11,485 4,594 3,719
0.095 1.250 75,000 30,000 3,361 13,443 5,377 4,213
0.109 1.250 75,000 30,000 3,961 15,843 6,337 4,776
0.120 1.250 75,000 30,000 4,455 17,822 7,129 5,207
0.134 1.250 75,000 30,000 5,117 20,468 8,187 5,742
0.035 1.500 75,000 30,000 918 3,671 1,469 1,367
0.049 1.500 75,000 30,000 1,311 5,243 2,097 1,896
0.065 1.500 75,000 30,000 1,779 7,117 2,847 2,487
0.083 1.500 75,000 30,000 2,333 9,333 3,733 3,136
0.095 1.500 75,000 30,000 2,719 10,878 4,351 3,559
0.109 1.500 75,000 30,000 3,188 12,754 5,101 4,043
0.120 1.500 75,000 30,000 3,571 14,286 5,714 4,416
0.134 1.500 75,000 30,000 4,079 16,315 6,526 4,881
0.148 1.500 75,000 30,000 4,610 18,439 7,375 5,336
0.035 1.750 75,000 30,000 781 3,125 1,250 1,176
0.049 1.750 75,000 30,000 966 3,864 1,546 1,434
0.065 1.750 75,000 30,000 1,505 6,019 2,407 2,146
0.083 1.750 75,000 30,000 1,965 7,860 3,144 2,711
0.095 1.750 75,000 30,000 2,284 9,135 3,654 3,080
0.109 1.750 75,000 30,000 2,668 10,672 4,270 3,504
0.120 1.750 75,000 30,000 2,980 11,921 4,768 3,832
0.134 1.750 75,000 30,000 3,391 13,563 5,425 4,242
0.148 1.750 75,000 30,000 3,817 15,268 6,107 4,645
0.165 1.750 75,000 30,000 4,357 17,430 6,972 5,124
0.035 2.000 75,000 30,000 680 2,720 1,088 1,032
0.049 2.000 75,000 30,000 966 3,864 1,546 1,434
0.065 2.000 75,000 30,000 1,303 5,214 2,086 1,887
0.083 2.000 75,000 30,000 1,697 6,788 2,715 2,387
0.095 2.000 75,000 30,000 1,968 7,873 3,149 2,715
0.109 2.000 75,000 30,000 2,294 9,175 3,670 3,092
0.120 2.000 75,000 30,000 2,557 10,227 4,091 3,384
0.134 2.000 75,000 30,000 2,901 11,605 4,642 3,751
0.148 2.000 75,000 30,000 3,257 13,028 5,211 4,111
0.165 2.000 75,000 30,000 3,705 14,820 5,928 4,542

 

CCanna

Q: Maidir le praghsanna feadánra cruach dhosmálta ASTM A269 TP304?

A: Athraíonn praghsanna ó raonta $ 5 go $ 7 in aghaidh an chileagraim, ag brath ar mhéid, tiús bhalla, soláthraí etc.

C: Cé chomh fada a thógann do chuid ama seachadta?

A: Tá an t-am seachadta laistigh de 5-21 lá

C: An bhfuil Seirbhís Shamplach ann?

A: Cuirtear samplaí ar fáil saor in aisce

C: Cad é an Cainníocht Ordú Íosta?

A: Gan Cainníocht Ordú Íosta

C: Conas na táirgí a phacáil?

A: Tá ciseal seachtrach páipéar uiscedhíonach ag an gciseal istigh agus socraítear é le pailléad adhmaid fumigation.

C: Tíortha Onnmhairithe

A: An Bhrasaíl, an Afraic Theas, an Indinéis, an India, Singeapór, an Mhalaeisia, an Iaráin, an Rúis, UAE, an tSile, Laos, etc

 

 

Clibeanna Te: 304 feadán cruach dhosmálta, feadán dhosmálta 304, astm a269 tp304, feadán ss304

Glaoigh Linn

whatsapp

Fón

R-phost